Description
4m Taulman 230 Nylon Filament 1.75mm Rep Rap MendelGreat for fixing clogged extruders or just want to test out Nylon Filament to see
if it will work with your machine.
Recommended Settings:
228-235C Extrusion Temperature
70-80C Bed Temperature with PVA based glue
Speed: 30-60mm/s
.20mm-.4mm layer heights
Comes loose not on a reel.
Nozzle Cleaning Steps:
1. Heat the nozzle to 200C
2. Run Nylon filament through the extruder
3. With Nylon in the nozzle, reduce the temperature to 135C, and once there let it sit for a minute
4. Slowly but firmly work the filament out of the top of the extruder
The key is to slowly work the filament out, millimeter by millimeter. You will know that you got the whole thing back out when you can see the narrow plastic that made it into the tip of the extruder.
If you pull too hard, or yank the filament too violently, it will break off inside the nozzle and you will have to repeat.
5. Repeat steps 1-4 until the filament you remove from the nozzle comes out clean
Not guaranteed to fix every clog